The following table provides an overview of selected materials and their relevant mechanical and technological properties. It serves as a basis for design, material selection, and evaluation in engineering and manufacturing processes. In addition to key parameters such as tensile strength and hardness, manufacturing-related aspects, certification requirements, and application-specific properties are also considered to ensure a reliable and traceable basis for decision-making.
| Material |
Properties |
| 1.4542 (17-4 PH)
[Condition H925, 4h at 496°C] |
- Corrosion-resistant stainless steel
- Tensile strength 1100 N/mm² (→ 1000 N/mm² with 10% reduction for design)
- Hardness 40–45 HRC (H925; “heat treatment: yes”)
- Ductile material
- IP68 achievable (laser weldable)
- 3.1 material certificate required per batch
- Impact energy at 20°C / 0°C / -20°C (provided by manufacturer)
- Use for diameters up to 50 mm
|
| 1.4418 + QT900
|
- Corrosion-resistant stainless steel
- Tensile strength 770 N/mm² (→ 700 N/mm² with 10% reduction for design)
- Hardness 35–40 HRC
- Ductile material
- 3.1 material certificate required per batch
- Impact energy at 20°C: K ≥ 60 J (provided by manufacturer)
- Impact energy at -20°C: K ≥ 42 J (provided by manufacturer)
|